OK 86.08 SMAW Type Basic
OK 86.08 deposits an austenitic manganese steel alloy which work-hardens under impact and compressive stresses. The electrode is primarily used for surfacing and building up manganese steel components such as crusher, jaws and hammers. The interpass temperature should be kept as low as possible. Welding current, A AC, DC+ OCV 70 V
|
|
Classifications | Approvals | Typical all weld metal composition | Typical properties all weld metal | | | | Redrying temperature, °C 200 Redrying time, hours 2 Recovery 105 Yield stress, MPa 480 Tensile strength, MPa 780 Elongation, % 20 Weld metal hardness, a w 180-200 HB Weld metal hardness, w h 44-48 HRC Machinability Grinding Metal-to-metal wear resistance Excellent Impact resistance Very good
Charpy V | Test temps, °C | Impact values, J | +20 | 70 | -20 | 45 | -40 | 35 | -60 | 25 |
|
Diameter, mm | 3,2 | 4,0 | 5,0 | Length, mm | 450 | 450 | 450 | Arc voltage, V | 23 | 23 | 25 | Welding current, A | 95-135 | 130-180 | 170-230 | N. Kg weld metal/kg electrodes | 0,60 | 0,60 | 0,60 | B. No. of electrodes/kg weld metal | 35,5 | 24,0 | 15,0 | H. Kg weld metal/hour arc time | 1,1 | 1,4 | 1,8 | T. Burn-off time, secs/electrode | 95 | 109 | 132 |
|
|