OK Tigrod 13.22 GTAW
A copper-coated, low-alloyed, 2.5% Cr, 1% Mo rod for the GTAW of creep-resistant steels of the same type. Also for welding low-alloyed high tensile strength steels. OK Tigrod 13.22 is normally welded with pure Ar as the shielding gas. The mechanical properties are given in the stress-relieved condition. Welding current, A DC(-)
|
|
Classifications | Approvals | Typical all weld metal composition | Typical properties all weld metal | SFA/AWS A5.28 | ER90S-G | DIN 8575 | W.nr 1.7384 | EN 12070 | W CrMo2Si | | |
| Sepros | UNA 046731 | |
UDT | EN 12070 | |
VdTÜV | | |
| C | 0,08 | Si | 0,7 | Mn | 1,0 | Cr | 2,6 | Mo | 1,0 | Wire composition |
| Yield stress, MPa >400StrRel 750º/0,5h Tensile strength, MPa >500StrRel 750º/0,5h Elongation, % >18StrRel 750°C/0,5h Elongation, % >18StrRel 750°C/0,5h
Charpy V | Test temps, °C | Impact values, J | +20 | 200StrRel 750ºC |
|
Diameter, mm | 1,0 | 1,6 | 2,0 | 2,4 | 3,2 | 4,0 | Length, mm | 1000 | 1000 | 1000 | 1000 | 1000 | 1000 | Weight of rods/box, kg | 5,0 | 5,0 | 5,0 | 5,0 | 5,0 | 5,0 |
|
|