OK Autrod 13.12 GMAW
A copper-coated, low-alloyed, 1% Cr, 0.5% Mo electrode for the GMAW of creep-resistant steels of the same type and other low-alloyed high tensile strength steels. OK Autrod 13.12 is usually welded with Ar/20CO2 as the shielding gas. The mechanical properties are given in the stress-relieved condition. Welding current, A DC(+)
|
|
Classifications | Approvals | Typical all weld metal composition | Typical properties all weld metal | SFA/AWS A5.28 | ER80S-G | EN 12070 | G CrMo1Si | GOST 2246 | 08X CM A |
| Sepros | UNA 485179 | |
UDT | DIN 8575 | |
VdTÜV | | |
| C | 0,1 | Si | 0,7 | Mn | 1,0 | Cr | 1,2 | Mo | 0,5 | Wire composition |
| Yield stress, MPa 670 Tensile strength, MPa 785 Elongation, % 18 Elongation, % 18 Werkstoff Nr. 1.7339
Charpy V | Test temps, °C | Impact values, J | +20 | 40 | 0 | 30 | -20 | 25 |
|
Diameter, mm | 0,8 | 1,0 | 1,2 | 1,6 | Arc voltage, V | 16-22 | 18-28 | 20-33 | 26-38 | Welding current, A | 40-170 | 80-280 | 120-350 | 225-480 | Wire feed, m/min | 2,0-10,8 | 2,7-14,7 | 2,7-12,4 | 3,1-12,0 | Deposition rate kg weld metal/hour | 0,4-2,6 | 1,0-5,4 | 1,5-6,6 | 3,3-11,6 |
|
|