OK Autrod 16.12 GMAW
A stainless ''ER308LSi'' electrode for the GMAW of corrosion-resistant steel containing approximately 19Cr10Ni and austenitic corrosion-resistant steel such as AISI 304, 304L. OK Autrod 16.12 is usually welded with Ar/(1-3%)O2 as the shielding gas. Welding current, A DC(+)
|
      |
| Classifications | Approvals | Typical all weld metal composition | Typical properties all weld metal | | SFA/AWS A5.9 | | ER308LSi | | EN 12072 | | G 19 9 LSi | | Werkstoffnummer | | ~1.4316 |
| | DB | 43.039.01 | |
| DNV | 308L MS (-60°C) | |
| Sepros | UNA 485178 | |
| UDT | DIN 8556 | |
| Ü | 43.039/1 | |
| VdTÜV | | |
| | C | <0,03 | | Si | 0,8 | | Mn | 1,7 | | Cr | 20,2 | | Ni | 10,0 | | Wire composition |
| Yield stress, MPa 370 Tensile strength, MPa 620 Elongation, % 36 Elongation, % 36
| Charpy V | | Test temps, °C | Impact values, J | | +20 | 110 | | -60 | 90 | | -196 | 60 |
|
| Diameter, mm | 0,6 | 0,8 | 0,9 | 1,0 | 1,2 | 1,6 | | Arc voltage, V | - | 15-24 | 15-28 | 15-28 | 15-29 | 23-29 | | Welding current, A | - | 55-160 | 65-220 | 80-240 | 100-300 | 230-375 | | Wire feed, m/min | - | 4,0-17 | 3,5-18 | 4,0-16 | 3,0-14 | 5,5-9 | | Deposition rate kg weld metal/hour | - | 1,0-4,1 | 1,1-5,4 | 1,5-6,0 | 1,6-7,5 | 5,2-8,6 |
|
|