OK Autrod 12.51 GMAW
A copper-coated, manganese-silicon bearing electrode for the GMAW of unalloyed steels, such as general structural steels with a minimum tensile strength of 530 MPa, and for fine-grained, carbon-manganese steels with a minimum yield strength of 420 MPa. OK Autrod 12.51 can be welded with Ar/20CO2 or pure CO2 as the shielding gas. The mechanical properties quoted here are welded with Ar/20CO2 as the shielding gas. Welding current, A DC(+)
|
|
Classifications | Approvals | Typical all weld metal composition | Typical properties all weld metal | SFA/AWS A5.18 | ER70S-6 | EN 440 | G3Si1 |
| ABS | 3SA, 3YSA | |
BV | SA3YM | |
CL | | |
DB | 42.039.06 | |
DNV | III YMS | |
DS | EN 440 | |
GL | 3YS | |
LR | 3 3YS | |
PRS | 3YS | |
RINA | SG 52 3 | |
RS | 3YMS | |
Sepros | UNA 485178 | |
SFS | EN 440 | |
SS | EN 440 | |
UDT | DIN 8559 | |
Ü | 42.039/1 | |
VdTÜV | | |
| C | 0,1 | Si | 0,9 | Mn | 1,5 | Wire composition |
| Yield stress, MPa 470 Tensile strength, MPa 560 Elongation, % 26 Elongation, % 26
Charpy V | Test temps, °C | Impact values, J | +20 | 130 | -20 | 90 | -30 | 70 |
|
Diameter, mm | 0,6 | 0,8 | 0,9 | 1,0 | 1,2 | 1,4 | 1,6 | Arc voltage, V | 15-20 | 18-24 | 18-26 | 18-32 | 18-34 | 22-36 | 28-38 | Welding current, A | 30-100 | 60-200 | 70-250 | 80-300 | 120-380 | 150-420 | 225-550 | Wire feed, m/min | 5,5-13 | 3,2-13 | 3,0-12 | 2,7-15 | 2,5-15 | 2,3-12 | 2,3-12 | Deposition rate kg weld metal/hour | 0,7-1,7 | 0,8-3,0 | 0,9-3,6 | 1,0-5,6 | 1,3-8,0 | 1,6-8,7 | 2,1-11,4 |
|
|