OK Tigrod 19.49 GTAW
Welding current, A DC(-)
|
|
Classifications | Approvals | Typical all weld metal composition | Typical properties all weld metal | SFA/AWS A5.7 | ERCuNi | EN 14640 | S Cu 7158 (CuNi30) |
| | C | <0,05 | Si | <0,1 | Mn | 0,8 | Fe | 0,6 | Cu | bal. | P | ³0,01 | S | ³0,01 | Ni | 31,0 | Al | ³0,03 | Pb | 0,007 | Ti+ | | Nb | 0,35 | | | Wire composition |
| Yield stress, MPa 180 Tensile strength, MPa 350 Elongation, % 40 Elongation, % 40
Charpy V | Test temps, °C | Impact values, J | +20 | 90 |
|
Diameter, mm | 1,6 | 2,0 | 2,4 | Length, mm | 1000 | 1000 | 1000 | Weight of rods/box, kg | 5 | 5 | 5 |
|
|